![](/resources/assets/images/mobile.png)
![河南美飾龍新材料有限公司](http://img3.dns4.cn/pic/281844/p3/20190527094134_2728_zs.jpg)
河南美飾龍新材料有限公司
主營產(chǎn)品: 真石漆
多彩真石漆批發(fā)-美飾龍-別墅多彩真石漆批發(fā)
價(jià)格
訂貨量(KG)
¥2.80
≥1
店鋪主推品 熱銷潛力款
祺祻祶祷祸祷祲祲祲祲祲
![](https://img.zhaosw.com/upload/images/348/696/e4adc7f2-9e71-4a18-8a31-d2bae7a304c6.jpg)
![](https://img.zhaosw.com/upload/images/348/696/1001fb5b-9e10-49fd-99a5-cb600f077495.jpg)
![](https://img.zhaosw.com/upload/images/348/696/1200135a-af5f-430b-a4d4-d4c7a4f8d160.jpg)
![](https://img.zhaosw.com/upload/images/348/696/1e07afef-3843-4eef-825c-ece923706afe.jpg)
![](https://img.zhaosw.com/upload/images/348/696/c478a147-4cd0-44d2-b507-6a3c7398a6a9.jpg)
![](https://img.zhaosw.com/upload/images/348/696/5b74313a-ec08-4d99-af2f-3cea1f41427a.jpg)
![](https://img.zhaosw.com/upload/images/348/696/db95ff1b-fbae-4f0a-9f92-ba0635ba2efa.jpg)
真石漆噴涂:
1、噴涂時(shí)浮點(diǎn)大小可用“槍塞”來調(diào)節(jié)控制,在 噴涂過程中,噴槍口中心線要始終與噴面垂直,噴槍斗與噴面距離為0.3-0.5m。按設(shè)計(jì)效果調(diào)節(jié)噴槍,使其氣壓和出料達(dá)到要求效果。
2、按分格為單位噴涂完整的工作面,收槍或中涂收工,必須噴涂完整的分格面,不允許噴涂一半就ting工,避免造成接痕。
3、在真石漆未干時(shí),用平滾筒滾壓一遍。噴涂一格,在石漆未干燥時(shí),及時(shí)揭掉分格粘膠帶。
真石漆噴涂施工后,在良好的天氣環(huán)境條件下,三天后涂層仍能用指甲摳動(dòng)的現(xiàn)象,稱之為涂層太軟。乳液選擇不當(dāng)或者乳液含量不足,造成漆膜成膜時(shí)涂層不夠緊密,是導(dǎo)致真石漆涂層發(fā)軟的主要原因。
解決方法是,選擇配制真石漆的專用乳液,其最di的成膜溫度不應(yīng)低于20℃。如果最di成膜溫度較高,可能會(huì)造成在氣溫較低時(shí)不易成膜,這可以通過適當(dāng)添加成膜助劑的方法來解決。適量的成膜助劑在涂層干燥后可基本揮發(fā)完,一般不會(huì)影響涂層的性能。
有些真石漆涂層在每次下雨以后,都會(huì)發(fā)白,涂層變得疏松,而在雨停后,經(jīng)太陽一曬,涂層又恢復(fù)原來的顏色。其實(shí),這是由于涂層的耐水性不好、吸收了水分所引起的,配方原因是選用的丙xi酸乳液在合成時(shí)需加入表面活性劑,有些廠家為了增加乳液的穩(wěn)定性,所用的表面活性劑大大超量;前面一段時(shí)間,有個(gè)施工隊(duì)的負(fù)責(zé)人來咨詢,他們負(fù)責(zé)的一個(gè)項(xiàng)目漆膜像紙一樣成片撕下,從發(fā)來的照片看,并不能說明漆不好,相反,能成膜連成一片的墻面漆反而是乳液含量比較高,漆的質(zhì)量比較好的。有些廠家在制備真石漆時(shí)加入羧甲ji纖維素等物質(zhì)作為增稠劑,以及加入ben甲酸鈉作為防腐劑。